WTF?
I pour a pail of blast rock in a classifier turn on a 2" fire hose that wet classifies it into an 80 gallon barrel, ad a half cup of surfactant turn on another jet to agitate and it pours into a sluice which captures the heavy particulate and sends the rest into a retainer. Wash the sluice to collect the concentrate, roast it to eliminate sulfites and smelt it, pour it in a cone mold, let it set and knock the gold and silver button off the bottom.
If you can lift a 140 lb. pail of dirt 6 ft in the air, water, gravity, science and fire do the rest.
The whole deal fun as fukk and pay pretty good too. As of today my little collection worth ~ 6% more than when I started, soon to be 30%.
I recommend the hobby to anyone that can lift 140 lbs 6 ft. up and turn on a tap. After about 10 pails go play golf.
I'm at about 8.2 g/ton AU and 7g/ton AG.
I'll improve when I select and crush my own, all sort of good ore here.
Thanks for asking kid!!